Carbide cutting tools in the production process need to avoid what it is possible to prevent cracking?
Carbide Tool There are four main areas:
1, knife row is problematic in itself. The following row blade knife blade thickness not less than 1.5 times the thickness (preferably greater than 2-fold).
2, welding blade should bake through (not too far), copper water flow to all the welding surface (that is, not Weld).
3, the cooling after welding to slow, it is best to use the sand after welding knife row covered up, 12 hours before use.
4. Do not water cooled sharpening process (can be air-cooled), do not put the blade grinding too hot.
We have good tools Changzhou is a professional manufacturer of carbide cutting tools manufacturers, more options please contact us!
- High-end manufacturing escort "M
- Characteristic Analysis of Stain
- Broad market of artificial intel
- Changzhou high performance milli
- Speeding up the Improvement of I
- Analysis of the Characteristics
- Made in China from "usable" to "
- Very good high-performance milli
- China 's new offshore oil seismi
- What are the precautions for the
- Dill |
- End Mill |
- Reamer |
- Special To...|
- TAPS Serie...|
- Machining |
联系人:薛小姐 138 6101 6292,付小姐 153 1256 7839